Scientific Reports · 2014 · 226 citations · 31 references
Natural SciencesMaterials EngineeringMaterials ScienceElectrochemical EngineeringElectrochemistryNanomaterialsBattery MaterialsBattery TechnologyElectrochemical Energy StorageElectrode MaterialsEnergy StorageNanoporous MaterialsAnode Material SelectionAnode PerformanceCarbon For Lithium-ion BatteriesLithium-ion BatteriesLithium-ion Battery MaterialsNanostructured Battery MaterialsPorous SiliconSilicon Anodes
Herein, porous nano-silicon has been synthesized via a highly scalable heat scavenger-assisted magnesiothermic reduction of beach sand. This environmentally benign, highly abundant, and low cost SiO₂ source allows for production of nano-silicon at the industry level with excellent electrochemical performance as an anode material for Li-ion batteries. The addition of NaCl, as an effective heat scavenger for the highly exothermic magnesium reduction process, promotes the formation of an interconnected 3D network of nano-silicon with a thickness of 8-10 nm. Carbon coated nano-silicon electrodes achieve remarkable electrochemical performance with a capacity of 1024 mAhg(-1) at 2 Ag(-1) after 1000 cycles.
31
Size-Dependent Fracture of Silicon Nanoparticles During Lithiation
Shan Huang, Scott X. Mao, Ting Zhu · ACS Nano · 2012 · 2.3K citations
A Yolk-Shell Design for Stabilized and Scalable Li-Ion Battery Alloy Anodes
Nian Liu, Hui Wu, Matthew T. McDowell et al. · Nano Letters · 2012 · 1.8K citations
Natural Sciences, Materials Engineering, Materials Science +17
Size Dependent Fracture of Silicon Nanoparticles during Lithiation.
Jianyu Huang, Xiaohua Liu, Li Zhong et al. · Nano Letters · 2011 · 1.3K citations