Philosophical magazine · 1960 · 112 citations · 21 references
EngineeringMaterials EngineeringMaterials ScienceElectronic MaterialsMetallurgyNuclear MaterialsDefects In Electronic MaterialsMetallic Nuclear MaterialsMetalsRadiation Damage In MaterialsRadiation-resistant MaterialsActivation EnergyImpurity PathwaysIrradiation DamageMetal Radiation DamageNeutron Damage EffectsNeutron Irradiation DamageTemperature Dependence Of Radiation DamageTungsten-based Materials
Abstract Residual electrical resistivity has been used as an index of the damage present in tungsten irradiated in a nuclear reactor at 4°K and 77°K. A comparison was made between four different types of specimen prepared from cold-drawn wire respectively annealed before irradiation at 2000, 1500, 800°c and not at all. A fifth type of specimen was prepared from wire in a different state of purity. Four stages of recovery have been identified. the first occurring below −170°c, the second between −170 and 350°c with an activation energy rising from 0.25 to 1.7 ev, the third between 350 and 450°c with a single activation energy, of 1.7 ev and the fourth above 450°c. Second-stage recovery was enhanced by the presence of cold-work, affected by impurities and in well-annealed samples after light irradiations it was suppressed. A comparison of recovery with that in other metals leads to the conclusion that vacancies in tungsten migrate at 400°c with an activation energy of 1.7 ev. The general suggestion is advanced that vacancy migration occurs in all metals at a temperature approximately 20% of the absolute melting point T m °K, with an activation energy roughly 5 × 10−6 T m , ev. Recovery in tungsten above −170°c is attributed to the release of interstitials from traps associated with impurity atoms and dislocation lines. The free interstitial is assumed to become mobile below −170°c. The resistance versus dose curve for cold-worked tungsten shows acceleration and this is considered as evidence for the action of spikes on the unstable arrays of vacancies produced by deformation. A quantitative theory of damage and recovery developed from the above model predicts the observed behaviour of the five types of tungsten specimen.
21
Quenched-in Lattice Defects in Gold
J.E. Bauerle, J. S. Koehler · Physical Review · 1957 · 253 citations
Isothermal Annealing Effects in Irradiated Copper
A. W. Overhauser · Physical Review · 1953 · 161 citations
Natural Sciences, Materials Science, Electronic Materials +13
Interpretation of the Quenching Experiments on Gold
J. S. Koehler, F Seitz, J.E. Bauerle · Physical Review · 1957 · 126 citations
Quenching of imperfections in aluminum
Warren DeSorbo, David Turnbull · Acta Metallurgica · 1959 · 113 citations
Natural Sciences, Materials Engineering, Materials Science +10
Low-Temperature Reactor Irradiation Effects in Metals
T. H. Blewitt, R. R. Coltman, C. E. Klabunde et al. · Journal of Applied Physics · 1957 · 105 citations