Abstract Single crystals of LiNbO 3 are grown by the flux method. Measurements are made in the temperature range 20 to 1170 °C of the dielectric constant ϵ, dielectric loss and relative thermal expansion ΔL l / l along the polar axis (the three‐fold axis x 3 ) and perpendicular to the glide plane ( x 1 ). A sharp maximum in ϵ corresponding to a decrease in volume is observed in the x 3 direction at 1140 °C. This temperature is assumed to be the Curie temperature of LiNbO 3 which corresponds to the transition from an electrically ordered state (ferro or ferrielectric, rather than antiferroelectric) into a paraelectrical state. The temperature dependences of ϵ and Δ l / l below the Curie temperature show several similar anomalies. Some of these anomalies may be due to phase transitions.