Etching of High Alumina Ceramics to Promote Copper Adhesion

J.G. Ameen, D. G. Mcride, George C. Phillips

Journal of The Electrochemical Society · 1973 · 13 citations · 0 references

Concepts

Abstract

shown in Fig. 2 characteristic of elemental metal. It is estimated that the air-formed oxide is approximately 20A thick. The sample was coated to a thickness of 0.O01 cm with a proprietary polybutadiene. The emission spec-trum did not differ significantly from that of the un-coated sample. The coating was cured at 200°C in air for 30 min and the spectrum shown in Fig. 3 was obtained. The coated sample was then exposed to air-saturated, 3 % sodium chloride for 48 and 84 hr. The spectrum of the sample exposed for 84 hr is given in Fig. 4 where it will be noted that the center peak characteristic of cobalt oxide has increased in relative intensity. A companion uncoated sample, yielding an initial spectrum similar to that of Fig. 1, was exposed to the sodium chloride solution for 60 rain. Approximately 26 % of the electrodeposit remained as elemental cobalt after this time, as determined from the spectrum in Fig. 5 and the gain in radioactivity of the solution. In the coated sample there was no loss of cobalt to the solution as indicated by the negligible radioactivity of the solution and the absence of any measurable change in the radioactivity of the solid. The uncoated sample lost approximately 11 % in activity during the 60 min exposure to NaC1. A summary of the data ob-tained in this demonstration experiment is given in