International Journal of Applied Ceramic Technology · 2012 · 45 citations · 30 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsMaterials CharacterizationCeramic TechnologyPorous CeramicsStructural CeramicsElastic ModulusFlexural StrengthOxidationPore Size EffectsPorous Ceramic MaterialsPorous Silicon CarbideSilicon Carbide CeramicsTemperature Dependence
Porous SiC ceramics were synthesized by oxidation bonding of compacts of commercial α‐ SiC powder at 1300°C. Different volume fractions of petroleum coke powder were used for variation of porosity of ceramics from 36% to 56%. The material exhibited variations of pore size from 3 to 15 μm, flexural strength from 5.5 to 29.5 MP a, and elastic modulus from 3.3 to 27.6 GP a. Air permeation behavior was studied at 26–650°C. At room temperature D arcian ( k 1 ) and non‐ D arcian ( k 2 ) permeability parameters vary from 1.64 to 18.42 × 10 −13 m 2 and 0.58 to 2.95 × 10 −7 m, respectively. Temperature dependence of permeability was explained from structural changes occurring during test conditions.
30
Synthesis of dense silicon-based ceramics at low temperatures
Ralf Riedel, G. Passing, Herbert Schönfelder et al. · Nature · 1992 · 350 citations
Oxidation bonding of porous silicon carbide ceramics
J. H. She, Zhen‐Yan Deng, J. DANIEL-DONI et al. · Journal of Materials Science · 2002 · 175 citations