Journal of The Electrochemical Society · 2010 · 38 citations · 39 references
EngineeringChemical EngineeringEnvironmental EngineeringElectrochemical EngineeringElectrochemistrySurface ScienceChemical OxidationElectrochemical CellsElectrochemical TreatmentFuel Cell MembranesFuel CellsSulfur ChemistryFuel Cell ContaminationMembrane DegradationMembrane PerformanceOperational Performance AnalysisOxygen Reduction ReactionPolarization CurvesSulfur PollutantsSulfur-bearing Species
Airborne sulfur contaminants (, , and COS) cause the performance of proton exchange membrane fuel cells (PEMFCs) to degrade because they adsorb to the Pt catalysts and modify reaction sites for oxygen reduction. Electrochemical methods can be used for PEMFC performance recovery by oxidizing adsorbed sulfur species on the Pt catalysts to sulfate at high potentials and then removing them as water-soluble anions at low potentials. We examine the effectiveness of five distinct methods for PEMFC performance recovery after 3 h of exposure to 1 ppm in air at and (7 psi) and relative humidity of . The methods are tested when the Pt surface is partially covered but not completely saturated with sulfur species. The methods include variations in the cathode potential and gas environment ( or air). In the optimum method, the cells are switched from normal operation to by electrochemically consuming in the air. The potential is then cycled between 0.09 and 1.1 V vs the potential at the anode to restore 97% of the platinum catalyst electrochemical surface area. This in situ cycling method returns the polarization curves of contaminated PEMFCs to their original performance in less than 3 min.
39