The origin of unique initial magnetization curves in Dy-substituted (Nd1−<i>x</i>, Dyx)2Fe14B (<i>x</i> = 0−1) sintered magnets

Kurima Kobayashi, Kimiko Urushibata, T. Matsushita, Takahiro Akiya

Journal of Applied Physics · 2012 · 13 citations · 10 references

Concepts

Abstract

The coercivities (Hc), saturation magnetizations (Js), and anisotropy constants K1 of (Nd1−x, Dyx)2Fe14B sintered magnets (x = 0 to 1.0) are determined using high magnetic field measurements up to about 8 MA/m. The Ha, Js, and K1 values of samples with x &amp;lt; 0.5 are similar to those obtained in previous studies using single crystals; the Hc values for the sintered magnets are reported here for the first time. The magnetization into the single-domain states (SDS) in Dy-substituted sintered magnets is completed in lower fields than with Dy-free magnets (for example, 0.64 MA/m in the x = 1.0 sample and 1.6 MA/m in the x = 0.25 sample). The volume fraction of magnetized SDS grains when applying fields less than the demagnetizing fields of the samples also increases with increasing Dy content, i.e., 22 vol. % for a Dy-free sample and 48 vol. % for a Nd-free sample. A characteristic magnetization behavior of large pinning-like magnetization curves appeared in samples that were initially magnetized in a direction perpendicular to the c-axis and successively magnetized in the parallel direction. The apparent pinning field increased with increasing Dy concentration and reached 2.8 MA/m for the Nd-free samples. The origin of this behavior is the tilting of the c-axis in the crystal grains of sintered magnets and the clear preference for crystal grains in Dy-substituted samples to form SDS grains.

References

10