Industrial & Engineering Chemistry Research · 2006 · 37 citations · 30 references
ArtsBiochemistryFermentation SciencePapermakingPulp BiologyCellulose ChemistryPulp PreparationEthanol AdditionLignocellulosic Biomass ConversionLignocellulosic Biomass PretreatmentLignocellulosic Biomass UtilizationOrganosolv PulpingPulp Process OptimizationPulping ProcessesTensile Testing
This paper will consider the influence of the autohydrolysis pretreatment on Paulownia fortunei L . woods to obtain a liquid phase (which can be used as a commercial source of organic reagents) and also a solid phase (which is valuable as raw material for pulping processes). Moreover, the influence of the operating conditions viz., ethanol concentration (20%−60%), temperature (150−180 °C), and pulping time (30−90 min) on the organosolv pulping (the initial liquor-to-solid ratio was 8:1, with 10% of soda and 0.5% of anthraquinone) of the obtained Paulownia fortunei L . solid after the autohydrolysis process has been considered to determine the best pulping conditions and characteristics of the solid phase. In that form, the yield, kappa number, glucan and lignin contents, and tensile index values of the resulting pulps and paper sheets have been studied. The optimum of solubilized components has been obtained at 190 °C (0.92 g/L glucose, 1.61 g/L xylose, 0.60 g/L arabinose, 0.93 g/L acetic acid, 0.047 g/L 5-hydroxymethylfurfural, 0.141 g/L furfural, and 14.66 g/L oligomers). Under these conditions, a suitable chemical composition of pulps and acceptable yield (38%), kappa number (45), and tensile index (28.87 N m/g) could be obtained through operation at high temperature (180 °C), short pulping time (30 min), and low ethanol concentration (20%).
30
L. A. Zadeh · Information and Control · 1965 · 66.1K citations
Neuro-fuzzy modeling and control
Jyh‐Shing Roger Jang, Chuen–Tsai Sun · Proceedings of the IEEE · 1995 · 2.3K citations