Surface Structure in Corundum: I, Etching of Dislocations

Robert J. Scheuplein, P. Gibbs

Journal of the American Ceramic Society · 1960 · 102 citations · 14 references

Concepts

Abstract

Triangular etch pits, corresponding to the intersection of individual edge dislocations with the surface, have been observed in corundum single crystals after about 5 minutes of immersion in boiling phosphoric acid. Dislocations of both the (0001), (1120) and (1210), (1010) slip systems (where reference is made to the slip plane and slip direction, respectively) have been detected by this method. Edge dislocations of the (0001), (1120) system etched on surfaces close to and including the (1011) and {2021} planes. Dislocations of the {1210}, (1010) systems etched on the basal (0001) plane. The orientation dependence and technique of etching is described. The agreement with the Nye formula and with some of the expected properties of dislocations is cited as evidence that individual edge dislocations are actually detected. Typical photomicrographs of the etched surface in as‐received, deformed, flame‐polished, and polygonized crystals are shown. The dislocation structure produced in basally deformed crystals was found to depend critically on the constancy of the temperature during deformation. Crystals held at 2000°C. during bending exhibited dislocations arrayed in rows in the slip planes in good agreement with the Nye formula. Crystals bent while cooling (quench‐bent) had about twice as many dislocations as predicted by the Nye formula and these were distributed randomly. The possibility of vacancy condensation as a method for dislocation generation in quench‐bent crystals is discussed.

References

14