Normalised fatigue and fracture properties of candidate titanium alloys used in the pressure hull of deep manned submersibles

Fang Wang, Weicheng Cui, Binbin Pan, Shen Yunsheng, Xiaoping Huang

Ships and Offshore Structures · 2013 · 17 citations · 6 references

Concepts

Abstract

AbstractThe current available design rules of submersible structures from ship classification societies are based on the philosophy of strength design. Nowadays, higher requirements have been made for improved safe and economic design and operation of the submersibles, and the material selection criterion has paid more attention to the synthetic properties of materials of interest including fatigue and fracture properties of materials. Titanium alloys with relatively high ductility are widely used in pressure hull of deep manned submersibles nowadays. Much work should be devoted to systematic investigation of properties evaluation for candidate titanium alloys for submersible structures. This paper gives experimental results of fatigue and fracture properties of two candidate titanium alloys potentially used in pressure hull of deep manned submersibles. Test results are discussed by normalisation considering strength of the material which is an effective way to evaluate fatigue and crack growth properties of two materials. And to save cost and material test time in the future, an improved crack growth rate model proposed by the authors is used for prediction and unification of wide range of their crack growth rates. The comparisons between test data and prediction curves agree very well, which validate that the improved crack growth rate model can be used for prediction and unification of crack growth property of Ti80 and TC4 ELI at different load ratios.Keywords: deep manned submersiblestitanium alloysfatigue lifefracture toughnesscrack growth rate AcknowledgementsThis work is supported by High-tech 863 program under the project of 'Development of a 4500 m deep manned submersible' (Project No. 2009AA093303), Fourth Term of '333 Engineering' Program of Jiangsu Province under the project of 'Fatigue and fracture performance of domestically produced high strength titanium alloys for the 4500 m deep manned pressure hull' (Project No. BRA2011116) and Youth Foundation of Jiangsu Province 'Study on the time-scale crack growth rate model used in fatigue life assessment of pressure hull of deep-sea submersibles' (Project No. BK2012095).Nomenclaturea=The modified crack length which is equal to re plus the actual crack lengthath=The threshold value of crack lengthB=Specimen thicknessE=Elastic modulus of the materialKCf=The fracture toughness under fatigue loadingKIC=Plane strain fracture toughnessKmax=Maximum stress intensity factorKmin=Minimum stress intensity factorKQ=The conditional fracture toughnessKt=The stress concentration factorNf=The failure load cyclesPmax=The maximum force in p-v curve of fracture toughness testPQ=The force at a 5% secant offset from the initial slope in p-v curve of fracture toughness testre=An empirical material constant of inherent flaw length of the order of 1 μmR=Load ratioW=Specimen widthY=A geometrical factor to calculate the stress intensity factorsΔK=The stress intensity factor rangeΔKeff=The effective stress intensity factor rangeΔKeffth=The threshold effective stress intensity factor rangeΔKth=The threshold stress intensity factor rangeΔKth0=The threshold stress intensity factor range under zero load ratioσa=The stress amplitudeσb=The ultimate strength of the materialσmax=The maximum stress levelσmin=The minimum stress levelσv=The 'virtual strength' of the material representing the material strength at limit of 'perfect' condition (re = 0)σy=The yield strength of the materialυ=Poisson's ratio

References

6