Macromolecules · 2000 · 55 citations · 44 references
Natural SciencesChemistryMaterials ScienceMaterials ChemistryPolymer ChemistryPolymer MaterialsPolymer CrystallinityPolymer FoamsPolymer Phase BehaviorPolymer PhysicsPolymer ThermodynamicsThermoplastic PolymersFoaming ProcessesFoamsMelting TemperatureMelting Temperature AnalysisMicrocellular FoamsSyndiotactic PolymerizationThermal PropertiesWide-angle X-ray Scattering
Crystalline stereocomplex formation of isotactic poly(methyl methacrylate) ( it -PMMA) and syndiotactic poly(methyl methacrylate) ( st -PMMA) induced by high-pressure CO 2 at pressures in the 5−35 MPa range and at temperatures in the 30−110 °C range was demonstrated by means of differential scanning calorimetry (DSC) and wide-angle X-ray scattering (WAXS) investigations as a function of treatment pressure, temperature, and the it -PMMA/ st -PMMA ratio. At a constant it -PMMA/ st -PMMA ratio, the melting temperature of the stereocomplexes was shown to increase with increasing treatment pressure and temperature. The amount of the stereocomplex formed by high-pressure CO 2 was found to be higher than that by thermal annealing in bulk. The heat of melting of the stereocomplex was the highest for the 1/2−1/1 it -PMMA/ st -PMMA ratio. Compared with amorphous PMMA, the crystalline stereocomplex induced by high-pressure CO 2 contributes to the superior morphology of the microcellular foams obtained. For the CO 2 -treated polymer, the average cell size decreases and the average cell density increases as the amount of the stereocomplex that was formed increases.
44