Natural SciencesMaterials EngineeringMaterials ScienceMaterials CharacterizationMechanical Behavior Of MaterialsStructural MaterialsCrystallization ProcessesSilicate MineralsCompressive StrengthCompressive Strength DevelopmentCrystalline Phase FormationCrystalline StructureCuringMicrostructureMicrostructure CharacterizationX-ray Diffraction Analysis
This study reports on the microstructure, compressive strength, and drying shrinkage of metakaolin (MK) based geopolymers produced by partially replacing MK by oil palm ash (OPA). The OPA was used as raw material producing different molar ratios of SiO₂/Al₂O₃ and CaO/SiO₂. The geopolymer samples were cured at 80°C for 1, 2, or 4 hours and kept at ambient temperature until testing. The compressive strength was measured after 2, 6, and 24 hours and 7 and 28 days. The testing results revealed that the geopolymer with 5% OPA (SiO₂ : Al₂O₃ = 2.88 : 1) gave the highest compressive strength. Scanning electron microscopy (SEM) indicated that the 5% OPA sample had a dense-compact matrix and less unreacted raw materials which contributed to the higher compressive strength. In the X-ray diffraction (XRD) patterns, the change of the crystalline phase after heat curing for 4 hours was easily detectable compared to the samples subjected to a shorter period of heat curing.
19