Design of Advanced Bainitic Steels by Optimisation of TTT Diagrams and T0 Curves

Francisca G. Caballero, María J. Santofimia, C. Capdevila, Carlos García-Mateo, Carlos García de Andrés

ISIJ International · 2006 · 101 citations · 17 references

DOIFull text

Open access

Concepts

TL;DR

Cementite limits conventional bainitic steel performance, but silicon can suppress its precipitation in medium‑carbon steels. The study aims to design and mechanically characterize carbide‑free bainitic steels with an optimized mixture of bainitic ferrite, retained austenite, and martensite. Thermodynamic and kinetic models were employed to propose seven 0.3 wt % C carbide‑free bainitic steels for manufacturing. All but the most alloyed grade exhibited identical carbide‑free upper bainite and retained austenite microstructures, with tensile strengths of 1600–1950 MPa, 4 % uniform elongation, >10 % total elongation, and room‑temperature toughness comparable to quenched‑and‑tempered martensitic steels.

Abstract

Cementite is responsible of the limited application of conventional bainitic steels, however it has been proof that cementite precipitation during bainite formation can be suppressed by the judicious use of silicon in medium carbon steels. In this work, thermodynamic and kinetic models were used to design steels with an optimum bainitic microstructure consisting of a mixture of bainitic ferrite, carbon-enriched retained austenite and some martensite. Using these models, a set of seven carbide free bainitic steels with a 0.3 wt% carbon content were proposed for manufacturing. The work presented here is concerned with the microstructural and mechanical characterisation of the steels manufactured. Except for the steel with the highest content of alloying elements, all the grades present the same microstructure composed of carbide-free upper bainite and retained austenite after hot rolling and a two-steps cooling. Their tensile strengths range from 1600 to 1950 MPa while keeping a uniform elongation equal to 4% and a total elongation over 10%. Regarding toughness at room temperature, they match quenched and tempered martensitic steels.

References