Journal of the Physical Society of Japan · 1974 · 100 citations · 8 references
Natural SciencesMaterials SciencePhysicsCondensed Matter PhysicsMagnetic MaterialsMaterials PhysicsAlloysAntiferromagnetic MaterialsAntiferromagnetismCrystallographyMagnetic Properties Of SolidsMagnetism In SolidsAtomic OrderingMagnetic PropertiesManganese-based IntermetallicsNeel TemperatureNéel TemperatureTetragonal DistortionTetragonal SystemTransition Metal Magnetism
Crystallographic and magnetic properties were studied in the disordered γ-phase Mn 1- x Ir x (0.05< x <0.35) alloys. In Mn rich alloys, tetragonal distortion with axial ratio c / a >1 occurs at a temperature below their Néel temperature, T N . The tetragonal distortion temperature, T d in the antiferromagnetic ordered state decreases rapidly with increasing Ir and the alloys with x >0.15 remain cubic down to low temperatures. On the other hand, T N increases with alloying Ir at a rate of about 9 K/at%Ir up to 730 K at x =0.25 and it is extrapolated to 500±20 K for fcc Mn. It was concluded that the anomalous rise of T N is not mainly attributed to atomic order nor to the enhancement of exchange interaction due to lattice expansion, but that the perturbation of band structure due to alloying leads to stronger magnetic interaction. A Cu 3 Au type atomic ordering in the vicinity of x =0.25 was found to raise the T N by about 200 K. The origin of tetragonal distortion is discussed.
8
Takemi Yamada, Nobuhiko Kunitomi, Yutaka Nakai et al. · Journal of the Physical Society of Japan · 1970 · 197 citations