Journal of Applied Physics · 1985 · 85 citations · 22 references
Natural SciencesMaterials SciencePhysicsCrystal StructureMaterials CharacterizationPolymer ChemistryCrystal ChemistryCrystalline MaterialsDielectric PropertiesFerroelectric MaterialsPiezoelectric MaterialsPolymer CrystallinityCrystal Structure-property RelationshipsCrystallinityCrystallinity AnalysisCrystallinity ChangesCrystallizationFerroelectric PropertiesPiezoelectric PropertiesPiezoelectricity
Piezoelectricity and ferroelectricity in 80 mol % vinylidene fluoride/20 mol % tetrafluoroethylene copolymers (VDF-TFE) were measured at various crystallinities. In order to control the crystallinity, the crystallization pressure was varied from 1 bar to 5 kbar. All the samples prepared by this method contain only form I crystals but with various crystallinity and crystal thickness. Especially, a band structure characterizing an extended chain crystal was observed in the sample crystallized under more than 4 kbar. Remanent polarization (Pr) obtained by the D-E hysteresis curve increases with the crystallinity, and the extrapolated Pr of 126 mC/m2 nearly coincides with the value of 140 mC/m2 calculated from the unit cell dimension and dipole moment. The coercive field (Ec) decreases with the crystallinity. This would be explained by the expansion of intermolecular distance and a decrease in the number of folds, which affect the rotation of dipoles under an electric field.
22
Electric-field-induced phase changes in poly(vinylidene fluoride)
G. T. Davis, John E. McKinney, M. G. Broadhurst et al. · Journal of Applied Physics · 1978 · 635 citations
Piezoelectricity and pyroelectricity in polyvinylidene fluoride—A model
M. G. Broadhurst, G. T. Davis, John E. McKinney et al. · Journal of Applied Physics · 1978 · 442 citations
Ferroelectricity in polyvinylidene fluoride
R. G. Kepler, Robert A. Anderson · Journal of Applied Physics · 1978 · 358 citations