Journal of Polymer Science Polymer Chemistry Edition · 1977 · 11 citations · 9 references
Natural SciencesChemistryMaterials ScienceOrganic ChemistryPolymer ChemistryPolymer MaterialsPolymer CharacterizationPolymer CrystallinityPolymer StructurePolymerization ChemistryPolymerization ProcessesThermogravimetric AnalysisPolyimidesSolubilitySolution PolymerizationThermal PropertiesThermal StabilityThermogravimetric CurvesThermogravimetric Data AnalysisViscosity
Abstract Aromatic polyimides were synthesized by polymerization of 1,4,5,8‐naphthalenetetracarboxylic dianhydride and 2‐dialkylamino‐4,6‐dihydrazino‐1,3,5‐triazines by a solution polymerization method followed by cyclodehydration. The polyimides had number‐average molecular weights over 13,000–16,000 or viscosity values of 0.23–0.65 dl/g. The x‐ray diffraction diagram of polyimide I showed a crystal pattern, but the pattern became less pronounced with increasing length of the polymer side chain, and thus polyimide V showed a typical amorphous pattern. Study of the thermal stability of the polyimides by thermogravimetric analysis showed that a steep weight loss occurred in the range 380–410°C. Among the polyimides, I had only poor solubility in organic solvent, while IV and V were soluble even in general organic solvents such as tetrahydrofuran and dioxane.
9