Phase characterization and mechanical and flame‐retarding properties of nano‐CaSO<sub>4</sub>/polypropylene and nano‐Ca<sub>3</sub>(PO<sub>4</sub>)<sub>2</sub>/polypropylene composites

Satyendra Mishra, Arindam Mukherji

Journal of Applied Polymer Science · 2006 · 16 citations · 18 references

Concepts

Abstract

Abstract An in situ deposition approach was used for the synthesis of nano‐CaSO 4 and nano‐Ca 3 (PO 4 ) 2 . The nanosize particles were confirmed with an X‐ray diffraction technique. Composites of polypropylene (PP) with 0.1–0.5 wt % nano‐ or commercial CaSO 4 or nano‐Ca 3 (PO 4 ) 2 were prepared. The transition from the α phase to the β phase was observed for 0.1–0.3 wt % nano‐CaSO 4 /PP and nano‐Ca 3 (PO 4 ) 2 /PP composites. This was confirmed by Fourier transform infrared. A differential scanning calorimetry analysis was carried out to determine the thermal behavior of the nanocomposites with increasing amounts of the nano‐CaSO 4 and nano‐Ca 3 (PO 4 ) 2 fillers. Increases in the tensile strength and Young's modulus were observed up to certain loading and were followed by a decrease in the tensile strength. A continuous decrease in the elongation at break (%) was also observed for commercial CaSO 4 and larger nano‐Ca 3 (PO 4 ) 2 . A decrease in the mechanical properties after a certain loading might have been due to the agglomeration and phase transition of PP in the composites. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 103: 670–680, 2007

References

18