Wavelength and pulselength dependence of laser conditioning and bulk damage in doubler-cut KH 2 PO 4

John J. Adams, Justin R. Bruere, M. Bolourchi, Christopher W. Carr, Michael D. Feit, Richard P. Hackel, D. Hahn, J. Jarboe, Lawrence Lane, Ronald L. Luthi,

Proceedings of SPIE, the International Society for Optical Engineering/Proceedings of SPIE · 2005 · 22 citations · 0 references

DOIFull text

Open access

Concepts

Abstract

An experimental technique has been utilized to measure the variation of bulk damage scatter with damaging fluence in plates of KH<sub>2</sub>PO<sub>4</sub> (KDP) crystals. Bulk damage in unconditioned and laser-conditioned doubler-cut KDP crystals has been studied using 527 nm (2&#969;) light at pulselengths of 0.3 - 10 ns. It is found that there is less scatter due to damage at fixed fluence for longer pulselengths. In particular, there is ~4X increase in fluence for equivalent scatter for damage at 2&#969;, 10 ns as compared to 0.30 ns in unconditioned KDP. The results for the unconditioned and conditioned KDP show that for all the pulselengths the scatter due to the bulk damage is a strong function of the damaging fluence (&#952;<sup>~5</sup>). It is determined that the 2&#969; fluence pulselength-scaling for equivalent bulk damage scatter in unconditioned KDP varies as &#964;<sup>0.30±0.11</sup> and in 3&#969;, 3ns ramp-conditioned KDP varies as &#964;<sup>0.27±0.14</sup>. The effectiveness of 2&#969; and 3&#969; laser conditioning at pulselengths in the range of 0.30-23 ns for damage induced 2&#969;, 3 ns is analyzed in terms of scatter. For the protocols tested (i.e. peak conditioning irradiance, etc.), the 3&#969;, 300 ps conditioning to a peak fluence of 3 J/cm<sup>2</sup> had the best performance under 2&#969;, 3 ns testing. The general trend in the performance of the conditioning protocols was shorter wavelength and shorter pulselength appear to produce better conditioning for testing at 2&#969;, 3 ns.