Analysis of internal corrosion in subsea oil pipeline

Mochammad Noer Ilman, Kusmono Kusmono

Case Studies in Engineering Failure Analysis · 2014 · 116 citations · 5 references

DOIFull text

Open access

Concepts

TL;DR

A subsea crude oil API 5L X52 steel pipeline failed after 27 years, with leaks occurring near an elbow where fluid flow and chloride‑rich water were implicated. The study aimed to determine the primary cause of the pipeline failure. Standard failure analysis was performed, including visual inspection, chemical and mechanical characterization, metallurgical examination with optical microscopy and SEM‑EDX, and a three‑electrode corrosion test. The investigation concluded that electrochemical corrosion combined with flow‑induced corrosion caused the failure.

Abstract

Failure of a subsea crude oil API 5L X52 steel pipeline which led to oil leakage has been reported to occur after 27 years in service. Some leaks were found to form at the bottom of the horizontal API 5L X52 steel pipeline near an elbow section which connected the pipeline to a riser. The present investigation aims to analyze the main cause of failure by conducting standard failure analysis methods including visual examination, chemical and mechanical characterizations, metallurgical examinations using optical microscopy in combination with scanning electron microscopy (SEM) equipped with energy dispersive X-ray (EDX) analysis and corrosion test using a three-electrode potential technique. Results of this investigation suggest that the cause of failure is electrochemical corrosion combined with mechanical process known as flow-induced corrosion. The failure mechanism is discussed with specific attentions are paid to fluid flow rate and chloride-containing water phase.

References

5