Shipboard polymerization of acrylic acid

J. J. Kurland, D. R. Bryant

Plant/Operations Progress · 1987 · 14 citations · 3 references

Concepts

Abstract

Abstract In 1975 glacial acrylic acid polymerized in a tank of the S.S. Alchemist four days from port. Vapor and liquid vented at high pressure for three hours. Retained acid was stable. Probably steam leaking into steam coils or a deadheaded pump caused overheating that set off polymerization.

References