Journal of Polymer Science Polymer Physics Edition · 1984 · 50 citations · 20 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials ChemistryPolymer ChemistryPolymer MaterialsAmorphous SolidsCrystallization AnalysisCrystallization ProcessesPolymer CharacterizationPolymer CrystallizationPolymer Physical ChemistryActivation EnergyAnnealingAnnealing Temperature EffectsCold CrystallizationCrystallizationCrystallization BehaviorCrystallization KineticsPolymer Crystallization Kinetics
Abstract A series of uniaxially drawn films has been prepared from isotropic, amorphous poly(ethylene terephthalate) (PET) by using solid‐state coextrusion below its T g . To evaluating the crystallization behavior of the coextrudates, the cold‐crystallization temperature T c , Crystallization rate constant k , and activation energy E a have been studied as a function of extrusion draw temperature and draw ratio. The rapid crystallization of highly oriented amorphous PET in extrudates was followed by a temperature‐programmed DSC technique. This avoids the marked precrystallization often found in samples brought to appropriate isothermal temperatures. With increasing extrusion draw ratio, T c shifts to lower temperatures, the first‐order crystallization rate constant k increases markedly (by two or three orders of magnitude) and E a decreases markedly. For undrawn samples annealing at temperatures below or near T g (50–70°C) does not lead to crystallization, but with increased annealing temperature both T c and E a decrease. In contrast, for extrusion‐drawn PET, both T c and E a increase with draw temperature. All these features are consistent with our previous correlations with molecular draw ratio and birefringence.
20
Crystallization of polyethylene terephthalate
Walter H. Cobbs, R. L. Burton · Journal of Polymer Science · 1953 · 246 citations
The crystallization of oriented poly(ethylene terephthalate)
Fred Smith, R.D. Steward · Polymer · 1974 · 108 citations
Natural Sciences, Materials Engineering, Materials Science +12