Chinese Physics Letters · 2004 · 19 citations · 15 references
Natural SciencesMaterials EngineeringMaterials ScienceElectronic MaterialsMaterials ChemistryMetallic MaterialsAlloysElectrical ConductivityMetal MaterialsMetalsCritical Current DensityCritical Current PerformanceCurrent DensityGrain-size ControlHigh-temperature SuperconductorsLow-carbon SteelMagnesium AlloysMicrostructure
Graphite doped MgB2−xCx (x = 0.00, 0.05, 0.10) wires were fabricated via the in situ powder-in-tube method in flowing argon by using low carbon steel tubes as the sheath materials. With the increase of graphite concentration, the amount of unreacted graphite in the core area increases, and the average grain size of MgB2 decreases. It is found that the critical current density Jc can be significantly improved by graphite doping. The MgB2 wire with x = 0.05 exhibits the best Jc value of 16710 A/cm2 at 6 K, 4.5 T, but the MgB1.9C0.1 wire has the highest Jc value of 2060 A/cm2 at 6 K, 8 T. It is suggested that the enhancement of Jc is due to not only the improvement of the microstructure features but also the introduction of pinning centres.
15
Superconductivity at 39 K in magnesium diboride
Jun Nagamatsu, Norimasa Nakagawa, Takahiro Muranaka et al. · Nature · 2001 · 6.4K citations
Strongly linked current flow in polycrystalline forms of the superconductor MgB2
D. C. Larbalestier, L. D. Cooley, M.O. Rikel et al. · Nature · 2001 · 945 citations · Full text
Carbon-substituted MgB2 single crystals
Physica C Superconductivity · 2003 · 227 citations · Full text
Natural Sciences, Materials Engineering, Materials Science +11