Journal of Applied Physics · 1966 · 11 citations · 1 references
Natural SciencesMaterials EngineeringMaterials ScienceMetallic MaterialsMetallurgyThin FilmsAlloysMagnetic AnisotropyMagnetic Properties Of SolidsMetalsThin Film Magnetic PropertiesThin-film MaterialsAnisotropyAnisotropy FieldFilm ThicknessIron-based AlloysNickel AlloysNickel-based AlloysResistivitySubstrate Temperature Effects
A number of commercially available high-permeability nickel-iron-base alloys with low values of coercive force, magnetostriction, and crystalline anisotropy are of potential interest as materials for thin-film memory elements. Because of their compositional complexity, however, films of these alloys are not easily prepared by vacuum deposition. By use of bias sputtering, thin films of Mumetal, Conetic AA, Supermalloy, and 4–79 Permalloy have been successfully prepared. The effects of substrate temperature (100°–400°C) and film thickness (500–1000 Å) on the properties of wall-motion threshold H0, anisotropy field Hk0, dispersion α90, skew β, magnetostriction, and sheet resistivity have been experimentally determined. In general, for the same thickness and substrate temperature, the high-permeability alloys show lower H0 and Hk0 than the binary 81% Ni-19% Fe alloy. The data show that the reduction is most pronounced in the molybdenum-containing alloys, less so in Conetic AA, and least in Mumetal. Molybdenum additions appear to be the most effective in inhibiting the rate of increase of dispersion with increasing H0/Hk0 ratio; e.g., a Supermalloy film was deposited with H0/Hk0=0.9 Oe/0.4 Oe and α90=4.5°.
1