Low-pressure decomposition of chrysotile as a function of time and temperature

P. A. Candela, C. D. Crummett, D. J. Earnest, M. R. Frank, Ann G. Wylie

American Mineralogist · 2007 · 45 citations · 22 references

Concepts

Abstract

Chrysotile from Thetford, Quebec, was heated at constant temperature in quench furnaces from 200 to 1000 °C for 4 to 720 h, and the products were analyzed by XRD and optical microscopy. XRD patterns for chrysotile from Thedford, Jeffrey Quebec, and New Idria, California, heated for up to 8 h at constant temperatures from 400 to 800 °C in hydrothermal diamond-anvil cells, were obtained at 300 s intervals by using synchrotron radiation.