Microstructural Coarsening During Sintering of Boron Carbide

S. L. DOLE, S. Prochazka, Robert H. Doremus

Journal of the American Ceramic Society · 1989 · 187 citations · 10 references

Concepts

Abstract

The sintering behavior of boron carbide was investigated with particular attention given to microstructure development at various stages in the sintering process. Hot‐pressing and pressureless sintering techniques were employed and the effects of heating rate, firing atmosphere, and composition were used to characterize the sintering behavior. Pressureless sintering at temperatures up to 2300°C produces only limited densification. Microstructural coarsening is responsible for this since it leads to conditions where densification is slow. Hot‐pressing and carbon additions suppressed coarsening and permitted densification to >95% of theoretical density.

References

10