Physical Review · 1963 · 70 citations · 24 references
Natural SciencesMaterials SciencePhysicsCondensed Matter PhysicsSolid State PhysicsThermodynamicsDefect ThermodynamicsHigh-pressure ThermodynamicsMetalsNanowiresPhase TransitionsThermal Properties Of MaterialsElectrical ResistivityGold NanostructuresPressure Dependence Of Electrical PropertiesResistive Heating EffectsTemperature Dependence Of ResistanceTemperature Effects On DecayVacanciesVacancy Formation
99.999% pure gold wires were resistance heated to 680\ifmmode^\circ\else\textdegree\fi{}C in a gaseous medium at pressures between 400 and 11 000 atmospheres and quenched by turning off the heating current. The temperature decayed exponentially with a half-life of 1.6\ifmmode\times\else\texttimes\fi{}${10}^{\ensuremath{-}2}$ sec. The logarithm of the quenched-in electric resistance $\ensuremath{\Delta}R$ decreased linearly with increasing pressure. From the pressure effect on $\ensuremath{\Delta}R$ an activation volume for vacancy formation at 680\ifmmode^\circ\else\textdegree\fi{}C of $\ensuremath{\Delta}{V}_{f}=(9.16\ifmmode\pm\else\textpm\fi{}0.68)\ifmmode\times\else\texttimes\fi{}{10}^{\ensuremath{-}24}{\mathrm{cm}}^{3}=0.53\ifmmode\pm\else\textpm\fi{}0.04$ atomic volume is derived, assuming that the quenched-in resistivity is due to the formation of single vacancies. In the pressure range investigated, $\ensuremath{\Delta}{V}_{f}$ is apparently independent of the pressure. Using $\ensuremath{\Delta}{V}_{f}$ and Bauerle and Koehler's relationship between resistivity and fractional volume change during recovery, the electric resistivity of vacancies is (1.8\ifmmode\pm\else\textpm\fi{}0.4)\ifmmode\times\else\texttimes\fi{}${10}^{\ensuremath{-}6}$ \ensuremath{\Omega} cm/at.% and the vacancy concentration after quenching from 680\ifmmode^\circ\else\textdegree\fi{}C at room pressure with 1.6\ifmmode\times\else\texttimes\fi{}${10}^{\ensuremath{-}2}$ sec half-life of the temperature decay is (2.4\ifmmode\pm\else\textpm\fi{}0.5)\ifmmode\times\else\texttimes\fi{}${10}^{\ensuremath{-}5}$. The present data are in good agreement with those reported by DeSorbo from a calorimetric study of quenched foil. The present defect concentration is about 50% of the value extrapolated to 680\ifmmode^\circ\else\textdegree\fi{}C from the data of Simmons and Balluffi, who obtained the vacancy concentration in thermal equilibrium near the melting temperature.
24
Direct observations of defects in quenched gold
J. Silcox, P. B. Hirsch · Philosophical magazine · 1959 · 430 citations
Mechanism for Self-Diffusion in Metallic Copper
H. B. Huntington, Frederick Seitz · Physical Review · 1942 · 295 citations
Quenched-in Lattice Defects in Gold
J.E. Bauerle, J. S. Koehler · Physical Review · 1957 · 253 citations
Progress in very high pressure research
D. M. Warschauer · Solid-State Electronics · 1961 · 205 citations