Industrial & Engineering Chemistry Research · 2009 · 23 citations · 0 references
Natural SciencesChemical EngineeringMaterials ScienceCatalysisInorganic ChemistryReaction EngineeringCatalyst CharacterizationCatalyst RegenerationCatalytic MaterialsCatalytic Reaction EngineeringIndustrial CatalysisSurface CatalysisAdditivesCatalytic CrackingContact Time EffectsFluid Catalytic CrackingMetal CatalystsSulfur Dioxide ReleaseSulfur Release DynamicsSurface Area
Mn,Mg,Al-spinels derived from hydrotalcite-like compounds with different Al/(M 2+ + Al) molar ratios (0.25 and 0.50) and Mn/Mg of 0.30 were evaluated as catalysts for SO x removal under conditions similar to those found in fluid catalytic cracking (FCC) units. For both samples, the maximum rate of SO x pickup took place in the first 5 min of reaction, which is an interesting feature since the contact time inside the FCC regenerator is about 5−10 min. As to the regeneration step, propane seems to be a less effective reducing agent than hydrogen since it favored the release of SO 2 as reduction product and shifted the reduction profile to higher temperatures. The results from XRD indicate that SO 2 was mainly fixed as MgSO 4, although the formation of MnSO 4 has been indirectly evidenced. The performance of both samples for SO x uptake and sulfur release was also evaluated in the presence of CO and NO and no adverse effect was observed. The obtained results suggest that Mn-containing spinels are promising additives for SO x removal.