Japanese Journal of Applied Physics · 1987 · 45 citations · 2 references
Natural SciencesChemistryMaterials ScienceElectrochemistryMaterials ChemistryThin FilmsElectrochemical CellsElectrochromic MaterialsElectrode KineticsElectrode MaterialsThin Film Electrical PropertiesThin-film MaterialsElectrochromic DevicesElectrochromic Thin FilmsGlass ElectrodesResponse TimeVoltage
The dynamic properties of a V 2 O 5 ECD cell prepared by the sol-get method are mentioned. The V 2 O 5 thin film was electrochemically deposited onto ITO glass from a poly-vanadic acid sol. The response time of the ECD cell was 2–20 seconds, depending upon the cell voltage. The repeating time was more than 8×10 4 times. It is possible to fabricate large-area ECD cells by this method.
2
Transition Metal Oxide Gels and Colloids
Jacques Livage, J. Lemerle · Annual Review of Materials Science · 1982 · 114 citations