Journal of the American Ceramic Society · 1997 · 52 citations · 9 references
EngineeringMaterials EngineeringMaterials ScienceJoiningMechanical Behavior Of MaterialsStructural MaterialsCarbon-carbon CompositesComposite MaterialsJoining Of Dissimilar MaterialsJoining ProcessesJoint StrengthStructural JointsComposite JoiningInterlayer MaterialsJoining TechniquesJoint Shear StrengthOptimum TemperatureShear Strength AnalysisShear TestingTemperature Optimum
The feasibility of joining of 3‐D carbon—carbon (C–C) composites by using B and TiSi 2 interlayers has been investigated. The optimum temperature for joining with a B interlayer was determined to be about 1995°C and that for joining with a TiSi 2 interlayer was about 1490°C. The shear strengths of the joints made at these optimum temperatures were found to increase with the shear testing temperature up to a point, followed by a decrease at higher temperatures. For C–C specimens bonded at 1995°C with a B interlayer, the maximum joint shear strength (average value 18.35 MPa) was observed at the test temperature of 1660°C. The shear strength of joints produced with a TiSi 2 interlayer showed a maximum at the test temperature of 1164°C, with an average value of 34.41 MPa. The B interlayers reacted with C–C composite pieces during joining, and the product of reaction was identified as B 4 C. In specimens joined with TiSi 2 interlayers, the reaction between TiSi2 and C did not go to completion, and the bond interlayer contained TiC, SiC, and TiSi 2 .
9
Chemically vapor deposited Ti3SiC2
Takashi Goto, T. Hirai · Materials Research Bulletin · 1987 · 310 citations
Natural Sciences, Materials Engineering, Materials Science +7