Enhancement of Cr<sup>4+</sup> Concentration in Y<sub>3</sub>Al<sub>5</sub>O<sub>12</sub> Crystal Fiber by Pregrowth Perimeter Deposition

Cheng‐Nan Tsai, Yen‐Sheng Lin, Kuang-Yao Huang, Yen-Sheng Lin, Chien‐Chih Lai, Sheng‐Lung Huang

Japanese Journal of Applied Physics · 2008 · 14 citations · 19 references

Concepts

Abstract

Chromium ions tend to diffuse outward during the laser-heated pedestal growth (LHPG) of Y3Al5O12 (YAG) crystal fiber, in which the average Cr4+ ion concentration decreases significantly after each diameter-reduction step. The Cr4+ ions are replenished using an electron gun to deposit Cr2O3 and divalent-ion oxide (CaO or MgO) on the source rod circumference before LHPG. It was observed that Ca2+ has better efficiency to diffuse into the source rod more efficiently than Mg2+ generating fewer defects and stacking faults. By CaO deposition and post growth annealing at 1350 °C under an oxygen environment, a 110% increase in Cr4+ concentration was obtained. The achieved Cr4+ concentration and the ratio of Cr4+ to total Cr were 1.76×1018 cm-3 and 5.5, respectively. The Ca,Cr:YAG crystal fiber can thus be used as an ultra broadband laser material and amplified spontaneous emitter.

References

19