British Corrosion Journal · 1970 · 11 citations · 15 references
Natural SciencesChemical EngineeringChemistryElectrochemistrySurface ChemistrySurface ScienceCorrosion MechanismsElectrochemical CorrosionElectrochemical KineticsElectrode KineticsIron OxidesElectrochemical ReactionsElectrochemical Surface ReactionsIron DissolutionMetal PassivityOxide Film FormationPassivation KineticsPassivitySurface Film Formation
When iron is passivated in chromate solutions in the pH range 7·5–1·0, an oxide film forms on the surface and thickens logarithmically with time. At pH ≤ 1·6, dissolution of iron takes place at a measurable rate that is considerably higher than the rate of oxide film growth at the same pH. The amount of iron in solution varies in a parabolic manner with time and the spontaneous dissolution current is given by log idiss = –0·84 pH + constant. The dissolution current of active iron in sulphuric acid solutions is related to the pH of the solution by the expression log idiss = –0·36 pH + constant.These relationships are interpreted in terms of electrochemical reactions occurring at the surface of the iron, when it is active in sulphuric acid solutions, or at the oxide/solution interface in chromic acid solutions, when the iron is passivated and so covered with a surface film of oxide.
15