Phase Evaluation in <scp> Al <sub>2</sub> O <sub>3</sub> </scp> Fiber‐Reinforced <scp> Ti <sub>2</sub> AlC </scp> During Sintering in the 1300°C–1500°C Temperature Range

Charles B. Spencer, J.M. Córdoba, N. Obando, Aaron R. Sakulich, Miladin Radović, Magnus Odén, Lars Hultman, Michel W. Barsoum

Journal of the American Ceramic Society · 2011 · 25 citations · 43 references

Concepts

Abstract

In this article, the reactivity of Ti 2 AlC powders, with 3 and 10 μm alumina, Al 2 O 3 , fibers during pressure‐assisted sintering is explored. Samples were fabricated by hot‐isostatic‐pressing ( HIP ed) or hot‐pressing ( HP ed), and characterized by X‐ray diffraction, differential thermal analysis, and electron microscopy—both scanning and transmission—equipped with energy dispersive X‐ray spectroscopes. Samples prepared at 1300°C were fully dense, with no apparent reaction between fiber and matrix. In samples HP ed to 1500°C, even pure Ti 2 AlC powders dissociated to Ti 3 AlC 2 according to: 2 Ti 2 AlC = Ti 3 AlC 2 + TiAl x ( l ) + (1‐ x ) Al ( l / v ), with x &lt; 1. More severe Al loss results in the formation of TiC y . The presence of the Al 2 O 3 fibers delayed densification enough to allow most of the Al and some of the Ti to escape into the vacuum of the hot press or react with the encapsulating glass during HIPing a resulting in a more intensive dissociation of the Ti 2 AlC . Although, in principle Ti 2 AlC can be reinforced with Al 2 O 3 fibers, the processing/use temperature will have to be kept below 1500°C, as, at that temperature the fibers, used here, sinter together.

References

43