Rare Metals · 2009 · 14 citations · 16 references
EngineeringMaterials EngineeringMaterials ScienceMetallic MaterialsMetallurgySolidificationAlloy SolidificationAlloysMicrostructure EvolutionRapid SolidificationSolidification KineticsSolidification MicrostructureAlloy Solidification BehaviorAlloy Solidification MicrostructureGrain Growth During SolidificationGrain Structure EvolutionMicrostructural Transition CriteriaSolidification BehaviorSolidification ParametersSolidification Pathways
Abstract Al‐20Si‐5Fe melt was rapidly solidified into particles and ribbons and then consolidated to near full density by hot pressing at 400°C/250 MPa/1 h. According to the eutectic‐growth and dendritic‐growth velocity models, the solidification front velocity and the amount of undercooling were estimated for the particles with different sizes. Values of 0.43−1.2 cm/s and 15–28 K were obtained. The secondary dendrite arm spacing revealed a cooling rate of 6 × 10 5 K/s for the particles with an average size of 20 μm. Solidification models for the ribbons yielded a cooling rate of 5 × 10 7 K/s. As a result of the higher cooling rate, the melt‐spun ribbons exhibited considerable microstructural refinement and modification. The size of the primary silicon decreased from approximately 1 μm to 30 nm while the formation of iron‐containing intermetallic compounds was suppressed. Supersaturation of the aluminum matrix in an amount of ∼7 at.% Si was noticed from the XRD patterns. During the hot consolidation process, coarsening of the primary silicon particles and precipitation of β‐Al 5 FeSi phase were observed. Evaluation of the compressive strength and hardness of the alloy indicated an improvement in mechanical properties due to the microstructural modification.
16
Rapid dendrite growth in undercooled alloys
J. Lipton, W. Kurz, R. Trivedi · Acta Metallurgica · 1987 · 619 citations
Natural Sciences, Materials Engineering, Materials Science +12