Polymer Testing · 1995 · 23 citations · 7 references
Natural SciencesMaterials EngineeringMaterials ScienceMaterials CharacterizationMechanical Behavior Of MaterialsStructural MaterialsComposite MaterialsFracture MechanicsFracture ToughnessGlass MaterialsMechanical CharacterizationStrength Of MaterialsCrack Analysis In GlassCrack InitiationFracture Of Composite MaterialsGlass Fracture BehaviorGlass Fracture ToughnessMechanical Properties Of GlassesMode I Crack InitiationPolyamide
Various grades of commercially available glass fibre reinforced and unfilled Polyamide 66 compounds were injection moulded into a complex mould geometry. Mode I fracture toughness was determined using compact tension specimens cut from the mouldings. Rapid photographic procedures were used to identify positively crack initiation. Fracture toughness was higher in the filled systems than in the unfilled compounds; KQ for the latter was approximately 4 MN m−32. However, there was only a slight variation between the short glass fibre (50%, w/w) and long glass fibre (50%, w/w) containing grades with KQ values (calculated using load (P5%) in ASTM E399) of 7.0 and 6.4 MN m−32, respectively. Using photography, it was found that P5% coincides with the force at crack initiation for unfilled P A66, while for the filled materials P5% and Pcrack initiation did not coincide. Crack-initiation force values of 17 to 27% greater than P5% for the short fibre material and 29 to 67% larger than P5% for the long fibre material were identified. However, these higher values of load to crack initiation were at variance with the LEFM theory and are therefore questionable.
7