Journal of The Electrochemical Society · 1991 · 22 citations · 0 references
Natural SciencesChemistryMaterials EngineeringInorganic ChemistryMaterials ChemistryPhysical ChemistryElectrochromic MaterialsElectrode-electrolyte InterfacesInterfacial ElectrochemistryRedox ChemistryRedox-active MaterialsThin Film OxidationAnodic OxidationAnodic Oxide FilmsElectrolytesOxide Film Formation
Ellipsometry is used to study the electrochromic processes which occur when anodically grown films of vanadium oxide are electrochemically reduced and subsequently reoxidized. Films up to 200 nm in thickness are grown by anodizing vanadium in acetic acid and acetone electrolytes. When the current is made cathodic, the outer surface of the film is reduced to , and as coloring proceeds a phase boundary sweeps inward across the film toward the vanadium substrate. An optical inflection is observed when the phase boundary reaches the substrate, and no additional hydrogen is electrochemically bonded into the structure past this point. A field equal to 20% of the anodizing field is required to move hydrogen through the colored phase, and hydrogen transport is the rate‐determining step for the coloring process. When the current is made anodic again, the film undergoes a three‐stage bleaching process before oxide film growth continues. The first and third stages are brief but affect the entire film. The first stage culminates in the re‐establishment of an oxide film at the electrolyte interface. The second stage proceeds by inward motion of a phase boundary, this time with a bleached layer of on the outside and the colored layer on the inside. A field approximately equal to the anodizing field is required to move hydrogen through the bleached layer, and hydrogen transport is the rate‐determining step. Oxygen will be mobile at the anodizing field unless its transport number is zero and is likely to be incorporated in the film in groups. The third stage of the bleaching process begins when vanadium ions start to enter the film from the substrate and ends when the oxygen‐to‐vanadium ratio returns to its stoichiometric value.