Fabrication of Low OH and Low Loss Fluoride Optical Fiber

Seiko Mitachi, Yasutake Ohishi, S. Takahashi

Japanese Journal of Applied Physics · 1984 · 11 citations · 8 references

Concepts

Abstract

Low OH and low loss fluoride optical fiber of 6.3 dB/km at 2.13 µm is obtained by dry processing technique. This is the lowest loss fluoride fiber yet reported. The OH peak at 3 µm is reduced to less than one-hundredth that of conventional fiber preparation.