Journal of Applied Polymer Science · 2006 · 12 citations · 5 references
Natural SciencesMaterials EngineeringMaterials SciencePolymer ChemistryPolymer EngineeringPolymer MaterialsComposite MaterialsDegree Of ConversionPolymer DegradationPolymer ProcessingThermoplastic PolymersThermosetsComposite Thermal DegradationDegradationDegradation AnalysisMass Loss RatesPhysical PropertiesPolymer Thermal DegradationResin CharacterizationThermal Properties
Abstract The thermal behavior of allyl PPO and its cured resin were investigated. In the allyl PPO curing process, the specific temperatures were T gel = 173.6°C, T cure = 225.4°C, and T treat = 237.7°C, and the activation energy ( E a ) was 122 kJ/mol. The average number of PPO molecular units between two crosslinking points was about 20. In the degradation process of cured allyl PPO resin, the temperature at which mass loss equaled 1% was much higher than 300°C. The E a for degradation was calculated as 125 kJ/mol, with a degradation fraction (α) in the range of 0.15–0.65, or 117 kJ/mol with an α of 0.10–0.90. The most probable mechanism function of decomposition of the cured allyl PPO resin was f (α) = 2(1 − α) 3/2 or g (α) = (1 − α) −1/2 − 1. The thermocompressed laminate of the allyl PPO blending with an additive resin (made from BDM and DP) exhibited the desired properties. ©2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 4111–4115, 2006
5
Reaction Kinetics in Differential Thermal Analysis
H.E. Kissinger · Analytical Chemistry · 1957 · 13K citations
Kinetic Parameters from Thermogravimetric Data
A. W. Coats, J. P. Redfern · Nature · 1964 · 6.8K citations
The thermal decomposition of oxalates
Xiang Gao, D. Dollimore · Thermochimica Acta · 1993 · 102 citations