Key engineering materials · 2004 · 12 citations · 2 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsInterface ScienceCeramic BondingCoating TechnologyCoatingsHigh-temperature MaterialsHigh-temperature OxidationSurface CoatingsBond StrengthCrack FormationInterfacial Oxide LayersOxidationOxidation BehaviorThermal Barrier BehaviorThermal Barrier CoatingsThermally Grown Oxides
It is well known, that thermally grown oxide (TGO) forms at the interface between the thermal barrier top coating (TBC) and the bond coating during service. In previous work, SEM images showed that the TGO layer contained at least two layers with different oxides. One layer was Al 2O 3, and the other was a mixed oxide of NiO, CoO, Cr 2O 3, and their spinels. It was supposed that a reason for macro-crack formation near an interface is due to a decrease in bond strength or to the formation of stress concentration sites caused by the formation of pores in the mixed oxide. In order to improve the bond strength, a modified bond coating material was developed, which is MCrAlY with Ce and Si added. Four- point bending tests were carried out to measure the bond strength of conventional TBC and of the modified TBC with MCrAlYCeSi bond coating. As a result, the TBC with modified bond coating had a bond strength superior to the conventional one. It is likely that the reason for the superior bond strength is due to a notable difference in oxidation behavior.
2
Spalling of the Surface Oxide Formed on Ni-20Cr Alloys with Small Additions of Cerium and Silicon
Yasutoshi Saitô, Katashi Kiriu, Takashi Kimura et al. · Journal of the Japan Institute of Metals and Materials · 1975 · 17 citations · Full text
Natural Sciences, Materials Engineering, Materials Science +17