On the Mechanisms of Chromium Electrodeposition

James P. Hoare

Journal of The Electrochemical Society · 1979 · 74 citations · 0 references

DOIFull text

Open access

Concepts

Abstract

Steady-state polarization measurements were made on Pt bead cathodes in N~-stirred solutions of Na,~CrO4, iNa2Cr2OT, and chromic acid. Three main regions can be distinguished: oxide reduction, H2 evolution, and Cr(VI) re-duction to Cr(III) or to black Cr or both. To obtain the black Cr deposit, a polychromate must be present and a low pH must be maintained. Steady-state polarization measurements were made on Pt bead cathodes in N2-stirred solu-tions of Na2CrO4 and Na2Cr207 to which Na2SO4 had been added and of chromic acid to Which Na2SO4 or H2SO4 had been added. These data indicate that the active catalyst is HSO4- ion which catalyzes only the reduction of the chromous products of the reduced cathode film. Bisulfate ion also acts as a blocking agent which inhibits electron transfer to chromium ions. A de-tailed mechanism for the reduction of Cr(VI) solutions to Cr metal is pro-posed. To prevent the formation of stable Cr(H20)6 +3 complexes, a cathodic film of chromic dichromate is formed with one end blocked by complexing with HSO4- ions. Decomposition of the film by reaction with H30+ ions pro-duces chromous hydroxide, the reduction of which to metallic Cr is catalyzed by HSO4- ions. By the concept of a distribution function of trichromate-bisulfate complexes, the narrow range of HSO4- ion concentrations which must be controlled to maintain successful Cr deposition is made under= standable. As early as 1856 (1), Geuter deposited metallic chromium from chromic acid solutions made from K2Cr207 and H2SO4. Between this time and 1920,