The Scientific World JOURNAL · 2014 · 148 citations · 37 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsNanomaterialsNanotechnologyInorganic MaterialsInorganic NanoparticlesNanomaterial CharacterizationNanomaterials SynthesisNanoparticle CharacterizationNanoparticle SynthesisBand GapCrystallite Size AnalysisMetal Oxide Nanoparticle SynthesisPhotoluminescenceSpherical MorphologyTitanium Dioxide NanoparticlesZirconiaZirconia Nanomaterials
We report synthesis of ZrO₂ nanoparticles (NPs) using microwave assisted chemical method at 80°C temperature. Synthesized ZrO₂ NPs were calcinated at 400°C under air atmosphere and characterized using FTIR, XRD, SEM, TEM, BET, and EDS for their formation, structure, morphology, size, and elemental composition. XRD results revealed the formation of mixed phase monoclinic and tetragonal ZrO₂ phases having crystallite size of the order 8.8 nm from most intense XRD peak as obtained using Scherrer formula. Electron microscope analysis shows that the NPs were less than 10 nm and highly uniform in size having spherical morphology. BET surface area of ZrO₂ NPs was found to be 65.85 m²/g with corresponding particle size of 16 nm. The band gap of synthesized NPs was found to be 2.49 eV and PL spectra of ZrO₂ synthesized NPs showed strong peak at 414 nm, which corresponds to near band edge emission (UV emission) and a relatively weak peak at 475 and 562 nm.
37
Direct oxidation of hydrocarbons in a solid-oxide fuel cell
Seungdoo Park, John M. Vohs, Raymond J. Gorte · Nature · 2000 · 1.9K citations
Sandra Luz Martínez Vargas, José Carlos López, Amaya Romero et al. · Industrial & Engineering Chemistry Research · 2010 · 1.7K citations
Ceramics ductile at low temperature
J. Karch, R. Birringer, H. Gleiter · Nature · 1987 · 922 citations
Natural Sciences, Materials Engineering, Materials Science +12