Thermodynamics of crystalline linear high polymers. III. Thermal breakdown of the crystalline lattice of polyethylene

Bernhard Wunderlich, Peter M. Sullivan, Tamio Arakawa, A. B. Dicyan, J. F. Flood

Journal of Polymer Science Part A General Papers · 1963 · 33 citations · 31 references

Concepts

Abstract

Abstract The thermal breakdown of the crystalline lattice of polyethylene grown by quenching from solution (dendrites) and by cooling slowly from solution (single crystals) and melt has been investigated as a function of heating rate. The dendrites showed strong reorganization at temperatures only little above the crystallization temperatures. Heating rates as fast as 20°C./min. could not avoid this reorganization. Heating rates between 10 and 20°C./min. were necessary to have a constant melting point for single crystals grown from solution. The measured melting points were proportional to the thickness and perhaps the density of the samples as determined by interference microscopy and by the density gradient column method. Surface free energy values calculated from the lowering of the melting points range from 81–96 ergs./cm. 2 . Literature values on specific heats and specific volumes of bulk samples allowed a discussion of the premelting behaviour of semicrystalline polyethylene. It is found that the defects frozen‐in below the glass transition temperature “grow” above 250°K. depending upon the overall crystallinity. This destroys the additivity of the specific heat as well as the specific volume. Correlation with NMR and dynamic mechanical loss measurements are attempted. The difference between melting and dissolution temperature in toluene (0.5–8.0 mg. polyethylene/g. toluene) for slowly cooled bulk as well as solution crystals was found to be 26°C., placing the maximum dissolution temperature of polyethylene crystals in toluene at 111°C.

References

31