Vitrification kinetics of pure metals

V. I. Motorin

physica status solidi (a) · 1983 · 17 citations · 19 references

Concepts

Abstract

A vitrification criterion for substances with continuous law of crystallization is obtained. The maximum thickness of a glassy layer for Ag, Cu, Ni, Pb is proved to be not greater than 10−7 to 10−8 m. The corresponding quenching rate is about 1011 to 1013 Ks−1. If the thickness of the molten overlay produced by pulse heating on the surface of a bulk sample is greater than a certain value lc, crystallization at the interface between solid and liquid phases is significant. In the opposite case an amorphous or microcrystalline layer with qualities close to the amorphouse layer is generated. For Ag, Cu, Ni, and Pb lc ≈︁ 10−7 to 10−8 m. [Russian Text Ignored.]

References

19