Journal of Prosthodontics · 2000 · 38 citations · 11 references
DentistryDental Biomaterials ScienceDental Materials ScienceDental MaterialsProsthodontic MaterialsSurface Properties Of Dental MaterialsDenture Base MaterialsDenture HygieneDenture ProcessingDenture Teeth MaterialsSurface Finish QualitySurface HardnessChemical Denture CleansersDenture Base ColorDenture Cleanser EfficacyHardnessLiner MaterialsSilicone Liner UseSilicone Surface CleaningSurface Texture Development
PURPOSE: The purpose of this study was to compare color, texture, and Shore A hardness of a resilient silicone denture liner with as-polymerized, roughened, or pumiced surfaces after treatment with perborate-, persulfate-, or hypochlorite-containing denture cleansers at 25 degrees or 55 degrees. MATERIALS AND METHODS: Fifty-eight specimens that each exhibited an as-polymerized, a roughened, and a pumiced area were exposed to 5 different commercially available perborate-, persulfate-, or hypochlorite-containing denture cleansers at 25 degrees or 55 degrees continuously for 4 (1/2) months. The solutions were replaced twice a day. Control specimens were soaked in water with no cleanser. Before and after the 4 (1/2) -month cleaning regimen, the color, hardness, and texture of resilient liner surfaces were evaluated using a color densitometer, a Shore A durometer (Shore Instrument & Mfg Co, Freeport, NY), and a surface profilometer, respectively. Differences among groups after the cleanser treatment were determined using a repeated measures analysis of variance (alpha = 0.05) and a Tukey's Honestly Significant Difference post hoc test. RESULTS: Roughened specimen surfaces after 25 degrees or 55 degrees cleanser treatment exhibited significant color loss with some perborate-containing cleansers compared with the control. Roughened specimens treated at 55 degrees with perborate-containing cleansers also exhibited significantly greater color loss than those treated with the persulfate-containing cleanser. With roughened surfaces, significantly greater hardness was found with some perborate-containing cleanser compared with a hypochlorite-containing cleanser after treatment at 25 degrees. No differences were observed in surface texture based upon cleanser treatment. CONCLUSION: After silicone resilient denture liner treatment with certain perborate-containing denture cleansers, a greater amount of components could leach from the liner leading to a loss of color if the liner surface is rough.
11