Advanced Materials · 2013 · 62 citations · 25 references
Natural SciencesMaterials EngineeringMaterials ScienceMetallic MaterialsNanomaterialsNanotechnologyInorganic NanoparticlesNanoparticle CharacterizationNanoparticle StabilityPlasmonic MaterialsPlasmonic NanomaterialsPlasmonicsNanoparticle Surface PlasmonicsNanoparticlesNoble Metal NanostructuresPlasmonic Material CharacterizationPlasmonic NanoparticlesPlasmonic Nanostructures
Reduced degradation (oxidation) of silver nanoparticles (NPs) is achieved by contacting Ag with immiscible Co NPs. The relative decay of the plasmon peak (plot) shows that pure Ag NPs (blue dashed curve) decay by 25% in ca 20 days, whereas AgCo NPs last about 10 times longer, requiring nearly five months for a similar decay (red solid curve). The TEM images for both Ag and AgCo were taken after 50 days of storage under ambient conditions. As a service to our authors and readers, this journal provides supporting information supplied by the authors. Such materials are peer reviewed and may be re-organized for online delivery, but are not copy-edited or typeset. Technical support issues arising from supporting information (other than missing files) should be addressed to the authors. Please note: The publisher is not responsible for the content or functionality of any supporting information supplied by the authors. Any queries (other than missing content) should be directed to the corresponding author for the article.
25
CRC Handbook of Chemistry and Physics
Devendra Leena P · Journal of Molecular Structure · 1992 · 9.4K citations
Natural Sciences, Chemistry, Physics +12
Spectroscopy of Single Hemoglobin Molecules by Surface Enhanced Raman Scattering
Hongxing Xu, Erik J. Bjerneld, Mikael Käll et al. · Physical Review Letters · 1999 · 2.4K citations