EngineeringMaterials EngineeringMaterials ScienceMaterials CharacterizationMechanical Behavior Of MaterialsStructural MaterialsCladding MaterialsDamage MechanicsFracture MechanicsFracture ToughnessStrength Of MaterialsWork HardeningCladding FailureCladding Failure MechanismsCladding-fuel InteractionExperimental Stress AnalysisFinite Element Fracture AnalysisStructural Performance Of CladdingTensile DeformationTensile Strain
The influence of hydride blister on cold worked stress relieved Zircaloy-4 cladding tubes fracture toughness at room temperature was studied using hoop tensile tests and plane strain tensile tests. The experimental macroscopic fracture stress and strain values and an elastic-plastic finite element analysis of the mechanical tests with the CAST3 M code were used to calculate the J-integral and estimate the fracture toughness for several blister depths from 120 to 240 μm.
16
Matthieu Le Saux, Jacques Besson, S. Carassou et al. · Engineering Failure Analysis · 2009 · 83 citations
Natural Sciences, Materials Engineering, Materials Science +14
Summary and Interpretation of the CABRI REP-Na Program
J. Papin, B. Cazalis, J. M. Frizonnet et al. · Nuclear Technology · 2007 · 80 citations