Sulfidation Behavior of an Iron‐Nickel Alloy

J. P. Orchard, David J. Young

Journal of The Electrochemical Society · 1989 · 19 citations · 0 references

Concepts

Abstract

An alloy containing 41 weight percent Ni was reacted at temperatures of 793, 888, and 938 K with flowing gas mixtures corresponding to equilibrium sulfur partial pressures in the range from . At 793 K the reaction product consisted of an inner compact layer of plus pentlandite overgrown by layers of pentlandite and Ni‐rich sulfide whiskers. Morphologies at the higher temperatures were similar except that pentlandite was absent. At all temperatures increases in the partial pressure led to a more compact scale morphology. The scale phases are shown to be consistent with local equilibrium, although the scale‐gas interface is not exactly at equilibrium because dissociation is slow. Reaction kinetics were irregular at 793 K, due to scale‐alloy separation, but parabolic at higher temperatures. Growth kinetics of the compact layer were parabolic and are shown to be consistent with and highly nonideal defect levels.