CORROSION · 2006 · 26 citations · 2 references
Natural SciencesMaterials EngineeringMaterials ScienceCorrosion ScienceMetallic MaterialsMetallurgyCorrosion MechanismsCorrosion Of SteelsCorrosion ResistanceIntergranular CorrosionPitting CorrosionStainless SteelsCarbide PrecipitationChromium Carbide PrecipitationChromium DepletionFerritic Stainless SteelsFerritic Steel CorrosionPitting Corrosion ResistanceSensitizationStainless Steel Corrosion
This work investigates the influence of sensitization conditions on pitting corrosion resistance of ferritic stainless steel UNS S43000 aged at 800°C between 10 min and 320 min. UNS S43000 steel is susceptible to intergranular corrosion after solution treatment at 1,160°C followed by water-quenching, as a consequence of the chromium depletion of the grain boundaries adjacent areas, due to chromium carbide precipitation during cooling. Isothermal treatments of 10 min at 800°C decrease the sensitization degree, and intergranular corrosion resistance is recovered after 20 min at 800°C. The solution-treated specimens have a high pitting potential in 3.5% sodium chloride (NaCl) solution compared to the same material treated at 800°C for 10 min. The resistance to pitting corrosion is reduced by chromium depletion associated with an increase of inter- and intragranular precipitation of chromium carbide. For treatments longer than 20 min at 800°C, the pitting corrosion resistance returns to the high level observed for the solution-treated condition, as a consequence of chromium redistribution that occurs after 20 min at 800°C. The scan rate used in potentiodynamic tests plays a minor role on the pitting potential, while a rougher surface leads to lower pitting potentials in all studied conditions.
2