Journal of Applied Physics · 2005 · 19 citations · 19 references
Natural SciencesMaterials EngineeringMaterials ScienceMagnetic MaterialsMetallic MaterialsMetallurgyAlloysAmorphous Magnetic MaterialsAmorphous MaterialsAmorphous SolidsFerromagnetic MaterialsNanocompositesAmorphous AlloysAmorphous Magnetic AlloysCoercivityMagnetic PropertiesMaximum Energy ProductNanocrystalline AlloysNanocrystalline Magnetic MaterialsNanocrystalline Magnets
Nanocomposite alloys of fct γ1-Fe(Co)Pt, fcc γ-Fe(Co)Pt, and Fe(Co)2B phases with good permanent magnet properties have been formed by melt spinning followed by annealing. An amorphous phase was formed for Fe56.25−xCoxPt18.75B25 (x=0–20) alloys by melt spinning. The thermal stability of the amorphous alloys increases gradually with increasing Co content. The structure crystallized by annealing for 900s at 785K consisted of fct γ1-Fe(Co)Pt, fcc γ-Fe(Co)Pt, and Fe(Co)2B phases, and their average grain sizes were about 20nm. The nanocomposite alloys exhibit good hard magnetic properties. As the Co content increases, the coercivity Hci increases, the remanence Br and maximum energy product (BH)max decrease. The Br, reduced remanence Mr∕Ms, Hci, and (BH)max were 0.96T, 0.83, 340kA∕m, and 102.2kJ∕m3, respectively, for the 0at.% Co alloy. Higher coercivity (426kA∕m) was obtained for the 20at.% Co alloy albeit with lower Br(0.68T), Mr∕Ms(0.80), and energy product (66.7kJ∕m3). The good hard magnetic properties for the low Pt-containing alloys are interpreted as resulting from exchange magnetic coupling between nanoscale hard fct γ1-Fe(Co)Pt and soft fcc γ-Fe(Co)Pt or Fe(Co)2B magnetic phase.
19
Stabilization of metallic supercooled liquid and bulk amorphous alloys
Akihisa Inoue · Acta Materialia · 2000 · 5.8K citations
F.R. de Boer, W.C.M. Mattens, R. Boom et al. · 1988 · 1.3K citations