Mechanical and biological properties of bioactive bone cement containing silica glass powder

Masahiko Kobayashi, Takashi Nakamura, Jiro Tamura, Hirokazu Iida, Hiroshi Fujita, Tadashi Kokubo, Takemi Kikutani

Journal of Biomedical Materials Research · 1997 · 39 citations · 23 references

Concepts

Abstract

Silica glass powder (SG-P) made by a fusing-quenching method was added as a second filler to a bioactive bone cement consisting of MgO-CaO-SiO2-P2O5-CaF2 apatite and wollastonite containing glass-ceramic powder (AW-P) and bisphenol-a-glycidyl methacrylate (Bis-GMA)-based resin, to achieve a higher mechanical strength and better handling properties in use. Five types of cement were used, containing different weight ratios of AW-P/SG-P (Group 1 = 100/0; Group 2 = 75/25; Group 3 = 50/50; Group 4 = 25/75; and Group 5 = 0/100) as filler, to evaluate the effect of SG-P content on the biological, mechanical, and handling properties. The total proportion of filler added to the cements was 85% w/w. The compressive, bending, and tensile strengths and fracture toughness of the cements increased with SG-P content. The viscosity of cements also increased with SG-P content, and every cement could be handled manually. The cements were evaluated in vivo by packing the intramedullary canals of rat tibiae. An affinity index was calculated for each cement; this was the length of bone directly apposed to cement expressed as a percentage of the total length of the cement surface. Histological examination of implanted tibiae for up to 26 weeks showed that the affinity indices decreased with SG-P content and that those of all the cement groups increased with time. At 26 weeks, Groups 1 and 2 had almost identical affnity indices (79% and 75%; no significant difference) but those of the other groups remained at <50%. Group 2 had better mechanical and handling properties than Group 1, and an SG-P content in the filler of no more than 25% w/w did not interfere strongly with the bioactivity of the cement.

References

23