Japanese Journal of Applied Physics · 2002 · 20 citations · 6 references
Natural SciencesMaterials EngineeringMaterials ScienceCeramic MaterialsCeramicsThin FilmsDielectric CeramicsElectrical Properties Of CeramicsFerroelectric CeramicsPiezoelectric MaterialsThin Film Electrical PropertiesThin-film MaterialsBarium Titanate CeramicsCompositionField-induced StrainFiring Temperature RegimesOptimum TemperatureOrthorhombic SystemStrain Effects On Ferroelectric PropertiesTemperature Optimum
BaTi1-xZrxO3 (x=0–0.1) thick films were prepared by a screen-printing method on Pt bottom electrodes using ceramic substrates in the firing temperature range from 1250°C to 1450°C. The dielectric, ferroelectric and electric-field-induced strain properties of the thick films were examined in comparison with those of bulk ceramics. The optimum firing temperature to obtain maximum remanent polarization was 1400°C for the thick films. The phase transition temperatures were controlled by varying composition x for the thick films as well as the bulk ceramics. The maximum remanent polarization of 14.4 µC/cm2 for the thick film was obtained at x=0.025 in the orthorhombic phase.
6